Annual production of 25,000 tons of carrier diatomite production line

Senxi Machinery Senxi Machinery

Product News Updated Saturday Mar 29 10:27:06 CST 2025

1. Work system

Filtration diatomite production line
Crushing - 8h/day, 5 days a week, 230 days a year
Acid leaching, filtering, washing, drying, calcining - 3×8h/day, 7 days a week, 350 days a year
Grinding, grading - 3×8h/day, 5 days a week, 230 days a year
Packaging, storage, shipment - 2×8h/day, 5 days a week, 230 days a year
Carrier diatomite production line
Crushing - 8h/day, 5 days a week, 230 days a year
Drying - 3×8h/day, 7 days a week, 350 days a year
Grinding, grading - 3×8h/day, 5 days a week, 230 days a year
Packaging, storage, shipment - 2×8h/day, 5 days a week, 230 days a year

2. Raw ore indicators

Specific gravity 0.7 to 0.9 T/m3,
Natural moisture = 10 to 30%, average value = 20%
Mohs hardness = 2-3

Chemical analysis:

SiO2

PAF

AI2o3

Fe2O3

CaO

MgO

Na2O

K2O

TiO2

P2O5

51-80

7-12

0,1-6

0.1-6

0,4-4

0.4-4

6-16

1,7-2

1.7-2

0,3-1,6

0.3-1.6

0,4-0,5

0.4-0.5

0,1-0,2

0.1-0.2

0,1-0,2

0.1-0.2

3. Product Outline

Filtration of diatomaceous earth 25,000 tons/year
Specific gravity = 0.1 tons/m3
Natural moisture = 1.5%
Particle size: coarse material = 15-74μm, medium material = 10-15μm, fine material = 0-10μm

Chemical analysis average

SiO2

AI2O3

Fe2O3

CaO

MgO

Na2O

K2O

TiO2

PAF

88,4

88.4

3,4

3.4

1,5

1.5

0,4

0.4

0,7

0.7

0,5

0.5

0,4

0.4

0,1

0.1

4

Carrier diatomaceous earth 25,000 tons/year
Specific gravity = 0.2-0.3 tons/m3
Natural moisture = -5%
Particle size: coarse material = 0-74μm, fine material = 0-10μm

Chemical composition

Si02

SiO2

AI203

AI2O3

Fe203

Fe2O3

CaO

MgO

PAF

58

3

1,5

1.5

13

2

12

4. Brief description of production process

Filtered diatomite production line

(1) Crushing
(2) Acid leaching and washing
(3) Drying
The filtered material (water content 30%) is conveyed to a rotary kiln (processing capacity 5t/h) by a conveyor for drying and calcining (temperature 700 to 1000℃), and then conveyed to an air cooler for cooling (temperature 250-300℃). The cooled material (water content 1.5%) is conveyed to the calcined diatomite storage bin.
(4) Grinding, grading, packaging

Carrier diatomite production line

(1) Crushing
(2) Drying
The crushed material (water content 20%) is conveyed to a rotary kiln (processing capacity 5t/h) by a belt conveyor for drying (dried to 5% moisture).
(3) Grinding, grading, packaging